Wagner SprayTech 525 Paint Sprayer User Manual


 
GB
10
TexPerfect Flexio 525
i
Important: Wipe o the nozzle and air cap regularly
to make sure they do not get blocked.
Undercoats, sealing primer
Select a distance of about 15-20 cm and a low ow rate.
Mansory paint, ne plaster, structured paint
Select a distance of 15-20 cm, depending on the desired spray jet width.
For masonry paint select a medium or high ow rate.
For ne plaster, the material ow should be adjusted to the grain size. When using
larger grain sizes (e.g. 1 mm) a high ow rate should be set.
Apply the masonry paint and ne plaster in a criss-cross movement (g. 9).
If necessary, spray another 1-2 layers (allowing the material to dry rst).
i
With ne plaster the nal result cannot be evaluated until it has dried. Therefore
wait about 20-30 minutes until the rst layer is dry before you start touching-
up the wall.
i
The ow rate for ne plaster is lower than when using undercoat.
You therefore work more slowly in order to attain an even application.
16. Interruption of Work
Turn the machine o.
With ne plaster, observe the maximum processing time (usually 20-30 minutes). If
the spray attachment is not used for a slightly longer period, clean it, as the material is
hard to remove once dry.
During longer breaks, vent the container by briey opening and then closing it again.
Clean nozzle openings after an interruption in operation.
17. Taking Out of Operation and Cleaning
Proper cleaning is the prerequisite for problem-free operation of the paint application
device. No warranty claims are accepted in case of improper or no cleaning.
Never hold the spray gun rear part under water or immerse it into liquids.
Clean the housing only with a moistened cloth.
i
With mansory paint, ne plaster, structured paint and undercoats we
recommend using warm water for cleaning.